Recoating While Refueling
Rehabilitating In-Service Fuel Tanks
From JPCL, February 2021
By David Hunter, Pond & Company, Inc.
When numerous fuel tanks at a U.S. Army base required recoating, the scope of work went beyond the typical tank-painting project, as the tanks had to remain full and operational during work. With inclement weather adding further challenges, this article will highlight how the contractors were able to plan and complete the work safely, on time and on budget....