From JPCL, October 2020

By Simon Daly, Hempel A/S


One of the major challenges facing equipment operators in the process industries is corrosion under insulation, and choosing the optimal coating for protection against CUI is a complex affair. This article will discuss different coating tests with the aim of defining which methods can be used to simulate CUI conditions in the laboratory, and how to evaluate a coating material’s performance under related conditions....


(Login to read the full article)
   