Ceramic Epoxy Coatings in Immersion

From JPCL, September 2018

By Ben Rowland, Induron Protective Coatings, Inc.


The term "ceramic epoxy coatings" refers to an epoxy binder with ceramic media used as a pigment/filler. This article explores ceramic epoxy coatings for use in water storage, wastewater and pipeline applications and examines properties and characteristics that differ from traditional epoxies used in these environments. ...