Refurbishment or Replacement?
Cost-Effective Solutions For Aging Water-Storage Tanks
From JPCL, May 2018
By Nick Bressler, World International Testing, Inc.
In order to bring the 92-year-old Alta Vista Standpipe up to current AWWA standards and achieve the owner’s long-term goals, refurbishment was selected over replacement. This article describes the factors that played a role in choosing repair over replacement and the courses of action taken....