Coatings Technology
Appearance vs. Functionality: The Zinc Coatings
From JPCL, November 2017
By JORDAN MCMILLEN, AMERICAN GALVANIZERS ASSOCIATION
Seven types of zinc coatings are commonly used for corrosion protection in building construction today, each with its own unique properties. This feature explores the differences between these zinc coating methods along with their aesthetic performance and typical useful environment to help determine which is most suitable for a particular project or environment....