From JPCL, October 2017

By Michael O. Woodward, Carboline Company


Surrounded by high-rise buildings and crossing the Miami River, the Miami Avenue Bridge spans a heavily utilized waterway for recreational crafts, cargo vessels and private yachts leading to and from the Atlantic Ocean. This case history describes recoating this bridge after the discovery of a catastrophic, intercoat delamination failure....


(Login to read the full article)
   

Tagged categories: Adhesion; Bridges; Case History; Coating selection; Cost-savings; Epoxy; Overcoating; Program/Project Management; Project Management; Specification; Waterjetting