The Development of Corrosion Resistant 2- and 1-K Waterbased Zinc-Rich Paints

From JPCL, August 2017

By Kenichi Nakamura, Roval, Japan; and Pascal Verbiest, Ph.D, EverZinc, Belgium


This article explains the formulation and performance of a waterbased (WB) zinc-rich paint, with 95-percent zinc content in the dry film, that is able to provide corrosion protection to steel equal to that of hot-dip galvanizing....