Successful Flooring Installation On Concrete
Beating The Odds
From JPCL, July 2017
By Fred Goodwin, Lori Proops and Richard First, BASF Corporation
The authors describe the many interrelated elements that must be simultaneously considered to achieve a successful installation of flooring over concrete. Examination of different options is necessary to ensure a balance between a satisfied owner, a profitable installation and something everyone involved can be proud of producing....