Offshore Wind Farms Successful Corrosion Protection and Effective Quality Management
From JPCL, December 2016
By Peter Kronborg Nielsen, FORCE Technology
Following an uncertain start, the present offshore coatings systems for wind farms have shown fine durability against the aggressive marine environment. In this article, positive features from the first wind farms with more than 15 years of service are described, as is the importance of quality management....