Building a Solid Foundation for Concrete Floor Coatings
A Guide to Inspection and Surface Preparation
From JPCL, November 2016
By Steven Reinstadtler, Covestro LLC
An attractive, durable concrete floor coating requires methodical preparation before applying the coating system of choice. Discover how proper inspection, repairs, cleaning and profiling contribute to a successful concrete floor project....