Painted Aluminum Failures in South Florida Exposure
From JPCL, October 2016
By Kirk R. Shields, Corrosion Probe Inc.
Painted aluminum exterior units are rapidly failing in South Florida — sometimes even before the new homes and condos are occupied. This article explores why many painted aluminum practices just don’t work in South Florida, and recommends solutions for building owners and specifiers....