Coating Evaluation Process for Municipal Manholes

From JPCL, September 2016

By Bob Murphy, Sherwin-Williams Protective & Marine Coatings


The author describes the evaluation protocol for coatings in aggressive sewer environments in two scenarios undertaken by a southwestern U.S. city....