Telecom Meets Water Tower
From JPCL, May 2016
By Christopher Wolfgram and Daniel J. Zienty, Short Elliott Hendrickson Inc.
More and more, telecommunications companies are using water towers as macro cell sites, mounting equipment onto handrail systems designed initially for access and maintenance. The authors present testing to determine the extent of potential heat damage to interior and exterior tank coating systems caused by welding additional bracing for telecom equipment....