Treating Exterior Concrete Walls with Coatings
From JPCL, April 2016
By Ray Tombaugh, KTA-Tator Inc.
Coatings applied to exterior concrete walls improve aesthetics, isolate and protect the concrete and the building interior from the environment, and make cleaning an easier task. The selection and use of several prominent coating types used on concrete walls are discussed in this article....