Corrosion Protection in Maritime Environments: Assessing Systems for Offshore Structures

From JPCL, March 2016

By Günter Binder, Federal Waterways Engineering and Research Institute (BAW)


The author compares the accuracy of laboratory test results to that of long-term tests in nature and discusses the creation of standards in order to prevent corrosion of offshore wind generating structures under very corrosive conditions with minimal environmental impact....