Equifinality: Specifying Performance

From JPCL, March 2016

By Troy Fraebel and Tony Ippoliti, The Sherwin-Williams Company


This article explains the balanced equifinality principle in specification — leaving materials and methods as open as possible (but restricting when necessary) to achieve long-term protection of an asset at a reasonable cost....


(Login to read the full article)
   

Tagged categories: Cost-savings; Life cycle; Quality Control; Sherwin-Williams; Specification; Specification writing; Tony Ippoliti; Troy Fraebel