The Curse of the Mummy: Mysterious Tank Lining Failures in WAC Vessels
From JPCL, February 2016
By Mike O’Donoghue, Ph.D., Vijay Datta, M.S., and Sean Adlem, International Paint LLC.; Jack Whittaker, Cenovus Energy Inc.; Doug Wade, NWS Inspection Ltd.; and Margaret Pardy, Mag Consulting Inc.
In this article, the authors outline discoveries made from forensic work to unravel epoxy lining failures in several water treatment weak acid cation (WAC) vessels....