Development of Materials and Process Metrics for High-Performance Abrasive Blast Surface Preparation

From JPCL, February 2016

By Robert Kogler and Laura Erickson, Rampart LLC


The authors describe ongoing work being conducted with the Center for Corrosion Science and Engineering and the U.S. Naval Research Laboratory, with the support of the Naval Sea Systems Command, in order to understand and refine variations in surface preparation and their effect on the subsequent performance of marine coatings....