The Importance Of Pattern Recognition In Failure Analysis
From JPCL, December 2015
By Dwight G. Weldon, Weldon Laboratories, Inc.
The author describes cases where recognizing patterns used in conjunction with standard laboratory test methods aided in determining the causes of premature coating failures....