Psymplified Psychrometrics

From JPCL, July 2015

By Robert Ikenberry, California Engineering Contractors, Inc., and Don Schnell, Polygon


by Robert Ikenberry, California Engineering Contractors, Inc., and Don Schnell, Polygon

The authors discuss the impact of humidity on surface preparation, coating application and cure; and explain how learning more about atmospheric moisture can help to achieve successful coating projects....