Testing + Evaluation
Keeping Coatings in the Game
From JPCL, February 2015
By Michael P. Reina, P.E., KTA-Tator Inc.
by Michael P. Reina, P.E., KTA-Tator Inc. | |
![]() |
Testing at five major-league baseball stadiums offers insights into paint performance....
|