Clues to a Coating Failure Avoiding Fading Paint
From JPCL, June 2014
By Jayson L. Helsel, P.E., KTA-Tator Inc.
Uneven paint at a retail store offers lessons for specifying high-performance paint.... (Login to read the full article)