When Undercover Agents are Tested to the Limit: Coatings in Action (CIA) and Corrosion Under Insulation (CUI) at High Temperature

From JPCL, March 2014

By Mike O’Donoghue, Ph.D., Vijay Datta, MS, Adrian Andrews, Ph.D., and Sean Adlem, International Paint LLC; Linda G. S. Gray, MSc, Coating Consultant; Tara Chahl and Nicole de Varennes, CET, RAE Engineering and Inspection Ltd.; and Bill Johnson, AScT, Acuren Group Inc.


by Mike O’Donoghue, Ph.D., Vijay Datta, MS, Adrian Andrews, Ph.D., and Sean Adlem, International Paint LLC; Linda G. S. Gray, MSc, Coating Consultant; Tara Chahl and Nicole de Varennes, CET, RAE Engineering and Inspection Ltd.; and Bill Johnson, AScT, Acuren Group Inc.

This article, the second in a series on coatings in action and corrosion under insulation, reports the results of accelerated laboratory tests to evaluate the performances of two coatings systems on both carbon steel and stainless steel pipes in the temperature range for CUI and at elevated temperatures approaching 600 C....
(Login to read the full article)

   

Join the Conversation:

Sign in to our community to add your comments.