High-Solids Epoxy Systems for Protective and Marine Coatings
From JPCL, February 2014
By Daniel Totev, Air Products and Chemicals Europe B.V., and Marcelo Rufo, Air Products Brasil Ltda.
by Daniel Totev, Air Products and Chemicals Europe B.V., and Marcelo Rufo, Air Products Brasil Ltda. | |
![]() |
This article reviews the basics of high-solids epoxy coatings compared to conventional epoxy technologies and describes the fundamental technical differences between the two....
|