Cargo Tank Coatings - A Stressful Environment
From JPCL, March 2013
By Trevor Parry, Coating Consultant, and Bill Woods, Marinspec Associates Ltd.
by Trevor Parry, Coating Consultant, and Bill Woods, Marinspec Associates Ltd. | |
![]() |
The authors identify some of the stresses that marine cargo tank coatings may face during their service lifetimes, and how these stresses relate to coating failures....
|