Repair The Building Before You Repair The Paint
From JPCL, January/February 2013
By Kevin J. Brown and Kenneth A. Trimber, KTA-Tator, Inc.
by Kevin J. Brown and Kenneth A. Trimber, KTA-Tator, Inc. | |
![]() |
Coating over cracks and spalls, without making the proper repairs first, may doom a coating system to premature failure, especially as the problem areas could be symptoms of larger structural issues within the building....
|