F-Files: Mechanisms of Failure
The case of…surprise blistering and rusting on a new tank lining system
From JPCL, July 2012
By James D. Machen, Senior Coatings Consultant, KTA-Tator, Inc. and Richard Burgess, Series Editor, KTA-Tator, Inc.
by James D. Machen, Senior Coatings Consultant, KTA-Tator, Inc. and Richard Burgess, Series Editor, KTA-Tator, Inc. | |
![]() |