Laboratory Investigations into the Edge Corrosion Protection Capacity of Organic Coatings
From JPCL, May 2012
By Sascha Buchbach, Dr. Peter Plagemann, Fraunhofer Institute for Manufacturing Technology and Applied Materials Research; and Dr. Andreas W. Momber, Muehlhan AG
by Sascha Buchbach, Dr. Peter Plagemann, Fraunhofer Institute for Manufacturing Technology and Applied Materials Research; and Dr. Andreas W. Momber, Muehlhan AG | |
![]() |
This article begins with a summary of the first part of a research study on how edge geometry and coating type affect the corrosion performance of organic coatings on edges, with particular attention to ballast seawater tank applications. The article then reports test results from the second part of the study, which concentrated on the effects of various treatment methods and tools on the performance of coatings on edges in ballast tanks....
|