Restoring and Protecting Bridge Piles
From JPCL, January 2012
By Carl W. Scheffel, P.E., and H. Michael Simpson, Fox Industries
by Carl W. Scheffel, P.E., and H. Michael Simpson, Fox Industries | |
![]() |
The authors describe the requirements for repair systems that would be effective on concrete, wood, or steel pilings to prevent deterioration; do not require maintenance; and provide an economical, long-term solution for all substrates....
|