New Barrier on the Block? Making the Case for Coatings on CMU

From JPCL, January 2012

By Joe Maty


by Joe Maty

Could conventional paint and coatings products, applied at quite conventional film thicknesses, function effectively as air-barrier materials?...
(Login to read the full article)

   

Tagged categories: Air barriers; Building Envelope; Concrete coatings and treatments; Concrete masonry units (CMU); Kevin Knight; National Concrete Masonry Association