Research News
Protecting Concrete on the Beijing-Shanghai Railway Bridge
From JPCL, December 2011
By Huang Weibo, Liu Xudong, Lu Ping, and Ma Xueqiang, Research Institute of Functional Materials, Qingdao Technological University, China.
by Huang Weibo, Liu Xudong, Lu Ping, and Ma Xueqiang, Research Institute of Functional Materials, Qingdao Technological University, China. | |
![]() |
The authors give a brief history of polyurea use in China, describe the Beijing-Shanghai High-Speed Railway and the polyurea specification for it, explain the project's major coating challenges, and describe the tests that led to a solution. The authors are with the Research Institute of Functional Materials, Qingdao Technological University, China.
...
|