Getting it Right: Treating the Headache of Water in Concrete/Masonry Walls

From JPCL, October 2011

By Jayson L. Helsel, P.E.


by Jayson L. Helsel, P.E.

Concrete and masonry materials occupy a prominent position in contemporary commercial building construction, and logic dictates that coatings and other treatments would play an important performance and aesthetic role in construction of this type....
(Login to read the full article)

   

Tagged categories: Concrete coatings and treatments; Concrete masonry units (CMU); Good Technical Practice; KTA-Tator; Masonry; Masonry waterproofing