Rethinking Recycling: Cal Poly Project Charts New Processing Route

From JPCL, July 2011

By Brian Brake, Fanny Moo and V.C. Bud Jenkins


by Brian Brake, Fanny Moo and V.C. Bud Jenkins

House paint is being recycled for many reasons. The first, and probably the best, reason is that if it is not, then valuable resources are lost to the world and to the economy....