Angels and Demons in the Realm of Protective Coatings: The Underworld of VOCs

From JPCL, April 2011

By Mike O’Donoghue, Ph.D.; V.J. Datta, MS; and Russell Spotten, International Paint, LLC


by Mike O’Donoghue, Ph.D.; V.J. Datta, MS; and Russell Spotten, International Paint, LLC

The authors examine the "angels and demons" that coatings with exempt solvents pose for surface preparation and the success or failure in immersion service. Potable water and petrochemical service are the focus of the internal linings discussion....