Rensselaer Polytechnic Research Group Says Nanoscale Coating Safely Eradicates MRSA Bacteria
From JPCL, October 2010
By Joe Maty
by Joe Maty | |
![]() |
Researchers at Rensselaer Polytechnic Institute (RPI) reported that they have created a nanoscale coating based on a naturally occurring enzyme that safely eradicates methicillin-resistant Staphylococcus aureus (MRSA), the bacteria responsible for antibiotic-resistant infections....
|