Blister Fix: Finding a Cause and Solution to a Common Defect

From JPCL, October 2010

By Jayson L. Helsel


by Jayson L. Helsel

Coatings applied to concrete and masonry substrates can exhibit a number of defects related to moisture. One such defect—blistering—is examined here, in a review of a case encountered in a major commercial building....
(Login to read the full article)

   

Tagged categories: Blistering; Concrete coatings and treatments; Good Technical Practice; Paint defects