Erecting a defense of the dry building

From JPCL, December 2009

By John Edgar, Sto Corp.


by John Edgar, Sto Corp.

Architects, specifiers, and contractors who specify and apply coatings as water-resistive and air-barrier components in wall assemblies will enhance their odds of success in keeping the building dry if they master an understanding of the "leak triangle." Also useful is an awareness of the Three 'D' approach - Deflect, Drain, Dry....
(Login to read the full article)

   

Tagged categories: Building Envelope