New Waterborne Fluoropolymer Resins for Ultra-Weatherable Coatings

From JPCL, December 2009

By Winn Darden and Bob Parker, AGC Chemicals Americas; and Naoko Sumi, Isao Kimura, Masakazu Ataku, and Takashige Maekawa, Asahi Glass Co. Ltd.


by Winn Darden and Bob Parker, AGC Chemicals Americas; and Naoko Sumi, Isao Kimura, Masakazu Ataku, and Takashige Maekawa, Asahi Glass Co. Ltd.

this article describes solvent-borne and waterborne FEVE resins as well as the potential uses of new FEVE dispersion resins in coatings for field application where high weathering properties are needed....
(Login to read the full article)

   

Tagged categories: Accelerated laboratory testing; Coating Materials; FEVE; Fluoropolymer; Fluorourethane; Performance testing; Resins; Solventborne coatings; Waterborne coatings; Weathering