Anodizing provides protection and aesthetic appeal to aluminum elements of buildings, including windows, doors, skylights, curtain walls, entrances, roof coping, panel systems, and ornamental work. The versatility, utility, and visual effects of this technology are discusses, along with important factors that should be considered in specification, application, and maintenance....