Concrete Protection and Decoration - A different slant on treatments for tilt-up
From JPCL, October/November 2007
By Lorella Angelini, BASF Building Systems
by Lorella Angelini, BASF Building Systems | |
![]() |
High-build coatings can provide decorative and protective advantages in applications to tilt-up concrete wall panels. Unique performance properties of these materials are highlighted....
|