Crash Course: Getting up to speed on penetrating parking-deck sealers
From JPCL, March/April 2007
By Gary Henry, PROSOCO
by Gary Henry, PROSOCO | |
The most commonly specificed penetrating, breathable sealers for parking decks come in three basic types: silane-based treatments, siloxane-based treatments, and blends of the two....
|