Case History
Case History: Aircraft Carrier Sails through Tank Maintenance Project
From JPCL, January 2008
In August 2006, the USS Abraham Lincoln aircraft carrier cruised into Puget Sound in Bremerton, WA, and docked in preparation for a massive tank blasting and coating project that was expected to take nearly six months to complete. Thanks in part to a sophisticated air distribution system and custom-built dessicant dehumidification systems, the carrier was ready to sail two weeks ahead of schedule....
|