The print version of the Directory includes listings for painting contractor companies located primarily in North America, but also around the world. Expanded details for each company—including contact information, web addresses, breadth of industry experience and specialty services—are available in...

2023 Annual Directory of Industrial Painting Contractors

The print version of the Directory includes listings for painting contractor companies located primarily in North America, but also around the world. Expanded details for each company—including contact information, web addresses, breadth of industry experience and specialty services—are available in...

The Future of Water Tank Interiors: The Recoating of the Norma Marshall Reservoir

by Paul Trautmann and Josh Skinner, Sherwin-Williams Protective and Marine

The authors outline how a 100%-solids epoxy lining system was chosen to replace existing polyurethane- and epoxy-based linings on a 4.8-million-gallon ground storage tank, and how successful application brought the storage tank into compliance with the new NSF/ANSI/CAN 600 standard more than a year ...

The Future of Water Tank Interiors: The Recoating of the Norma Marshall Reservoir

by Paul Trautmann and Josh Skinner, Sherwin-Williams Protective and Marine

The authors outline how a 100%-solids epoxy lining system was chosen to replace existing polyurethane- and epoxy-based linings on a 4.8-million-gallon ground storage tank, and how successful application brought the storage tank into compliance with the new NSF/ANSI/CAN 600 standard more than a year ...

Polymer Coatings for Restoring Wastewater Treatment Plant Structures

by Hunter Sansone, A&W Coatings

This article recaps a project that involved rehabilitation of the headworks grit processing system and influent channel at the South Wastewater Treatment Plant in Brownsville, Texas. The author explains how properly selected and applied epoxy coatings were used to successfully complete the project.

Polymer Coatings for Restoring Wastewater Treatment Plant Structures

by Hunter Sansone, A&W Coatings

This article recaps a project that involved rehabilitation of the headworks grit processing system and influent channel at the South Wastewater Treatment Plant in Brownsville, Texas. The author explains how properly selected and applied epoxy coatings were used to successfully complete the project.