JPCL December 2015
SSPC 2016 featuring GreenCOAT will be held January 18–21 at the Henry B. Gonzalez Convention Center in San Antonio, Texas. The SSPC 2016 Advance Program is published to help protective and marine coatings professionals begin planning their activities at the conference and exhibition.
SSPC 2016 featuring GreenCOAT will be held January 18–21 at the Henry B. Gonzalez Convention Center in San Antonio, Texas. The SSPC 2016 Advance Program is published to help protective and marine coatings professionals begin planning their activities at the conference and exhibition.
The authors will discuss the key details in OSHA’s recently issued Standard for Confined Spaces and describe ways in which contractors and owners can assure compliance and safety when working in confined spaces.
The authors will discuss the key details in OSHA’s recently issued Standard for Confined Spaces and describe ways in which contractors and owners can assure compliance and safety when working in confined spaces.
This article discusses testing carried out on zinc-rich primers where part of the zinc metal dust was replaced by a conductive ferro-phosphorus alloy pigment and assesses the anti-corrosion performance and cathodic protection capabilities of the formulation.
This article discusses testing carried out on zinc-rich primers where part of the zinc metal dust was replaced by a conductive ferro-phosphorus alloy pigment and assesses the anti-corrosion performance and cathodic protection capabilities of the formulation.
The author describes cases where recognizing patterns used in conjunction with standard laboratory test methods aided in determining the causes of premature coating failures.
The author describes cases where recognizing patterns used in conjunction with standard laboratory test methods aided in determining the causes of premature coating failures.