JPCL November 2015


Meeting Demands of Gas Exploration: The Evolution of Pipeline Coatings

by E. Bud Senkowski, P.E., P.C.S., KTA-Tator, Inc.

This article describes the coating materials, surface preparation requirements and application methods used to protect gas pipelines. It also provides information about the types of polymer-based coatings that are both cost-effective and have a high level of acceptance in the gas pipeline industry.

Meeting Demands of Gas Exploration: The Evolution of Pipeline Coatings

by E. Bud Senkowski, P.E., P.C.S., KTA-Tator, Inc.

This article describes the coating materials, surface preparation requirements and application methods used to protect gas pipelines. It also provides information about the types of polymer-based coatings that are both cost-effective and have a high level of acceptance in the gas pipeline industry.

Nontoxic Barnacle Antifouling

by Brian Goldie, JPCL

Producing surfaces with high resistance to marine fouling and a high level of barnacle protection is key to a successful antifouling paint. The author discusses antifouling coating technology that has the potential to cut fuel costs and reduce greenhouse gas emissions.

Nontoxic Barnacle Antifouling

by Brian Goldie, JPCL

Producing surfaces with high resistance to marine fouling and a high level of barnacle protection is key to a successful antifouling paint. The author discusses antifouling coating technology that has the potential to cut fuel costs and reduce greenhouse gas emissions.

Close Encounters of the Third "Crude-Oil" Kind

by Mike O'Donoghue, Ph. D. and Vijay Datta, M.S., International Paint LLC

The authors compare and contrast the accelerated laboratory autoclave performance of various types of epoxy linings for tank, vessel and pipe spool applications in the oil and gas industry.

Close Encounters of the Third "Crude-Oil" Kind

by Mike O'Donoghue, Ph. D. and Vijay Datta, M.S., International Paint LLC

The authors compare and contrast the accelerated laboratory autoclave performance of various types of epoxy linings for tank, vessel and pipe spool applications in the oil and gas industry.

Awards and Special Events at SSPC 2016

This section will preview the variety of special events, including SSPC’s Annual Business Meeting and Awards Luncheon, scheduled to take place during SSPC 2016 featuring GreenCOAT at the Henry B. Gonzalez Convention Center in San Antonio, Texas from January 18 to 21, 2016.

Awards and Special Events at SSPC 2016