The authors will explain the methods and processes of slip coefficient and tension creep testing on steel bridges, buildings, and other structures that may contain bolted connections.
The authors will explain the methods and processes of slip coefficient and tension creep testing on steel bridges, buildings, and other structures that may contain bolted connections.
This article is focused primarily on very fast-cure, solvent-free polyurethanes, polyureas, and polyurethane/polyurea hybrid technologies, many of which are well-suited for immersion service. The chemistry, cure mechanism, safety aspects, strengths, and weaknesses of each technology will be discusse...
This article is focused primarily on very fast-cure, solvent-free polyurethanes, polyureas, and polyurethane/polyurea hybrid technologies, many of which are well-suited for immersion service. The chemistry, cure mechanism, safety aspects, strengths, and weaknesses of each technology will be discusse...
SSPC 2014 featuring GreenCOAT will be held Feb. 10–13 at Disney’s Coronado Springs Resort in Lake Buena Vista, FL. This article is a list of updates to the SSPC 2014 Advance Program that were received after it was published in the December 2013 JPCL.