JPCL November 2013


Laboratory Evaluation of Metalized Coatings for Use on Reclamation Infrastructure

by Dr. David Tordonato, P.E., and Dr. Allen Skaja, P.C.S., U.S. Bureau of Reclamation

The authors discuss the use of metalizing, or thermal spray coating (TSC) application, for corrosion protection on hydraulic structures. The article provides a background on metalizing, including previous research findings, and describes the U.S. Bureau of Reclamation’s most recent research findings...

Laboratory Evaluation of Metalized Coatings for Use on Reclamation Infrastructure

by Dr. David Tordonato, P.E., and Dr. Allen Skaja, P.C.S., U.S. Bureau of Reclamation

The authors discuss the use of metalizing, or thermal spray coating (TSC) application, for corrosion protection on hydraulic structures. The article provides a background on metalizing, including previous research findings, and describes the U.S. Bureau of Reclamation’s most recent research findings...

Understanding the Basics of Chemical-Resistant Polyesters and Vinyl Esters

by Gary Hall, Consultant

This article, the eighth in JPCL’s 2013 series on generic coating types, describes the basic chemistry of polyesters and vinyl esters, as well as properties, concerns with the materials, and application methods.

Understanding the Basics of Chemical-Resistant Polyesters and Vinyl Esters

by Gary Hall, Consultant

This article, the eighth in JPCL’s 2013 series on generic coating types, describes the basic chemistry of polyesters and vinyl esters, as well as properties, concerns with the materials, and application methods.

Take Part in SSPC 2014’s Special Events, Awards

SSPC 2014 featuring GreenCOAT will be held at the Coronado Springs Resort in Lake Buena Vista, FL, Feb. 10–13, 2014. This article previews the special events and awards ceremonies that will be offered to attendees and their guests, including the opening and closing ceremonies, spouse and guest tours...

Take Part in SSPC 2014’s Special Events, Awards

SSPC 2014 featuring GreenCOAT will be held at the Coronado Springs Resort in Lake Buena Vista, FL, Feb. 10–13, 2014. This article previews the special events and awards ceremonies that will be offered to attendees and their guests, including the opening and closing ceremonies, spouse and guest tours...