JPCL May 2013


Developments in Zinc Primers for Corrosion Protection

by Pascal Verbiest, dr.sc., Umicore Zinc Chemicals

The author reviews the different types of zinc powders and how they are made, types and compositions of zinc primers, suitable uses of these primers, and tips for application.

Developments in Zinc Primers for Corrosion Protection

by Pascal Verbiest, dr.sc., Umicore Zinc Chemicals

The author reviews the different types of zinc powders and how they are made, types and compositions of zinc primers, suitable uses of these primers, and tips for application.

Is Lead Dead? A Look Back and a Look Forward at 20 Years of Bridge Painting Under the OSHA Lead in Construction Interim Final Rule and Other Related Standards

by Alison B. Kaelin, CQA, ABKaelin, LLC

This article provides reports on statistics and violations of OSHA’s standard for protecting construction workers from lead exposure, summarizes findings on blood lead levels and health risks related to lead exposure, reviews OSHA 29 CFR 1926.62 and other lead exposure-related regulations, and offer...

Is Lead Dead? A Look Back and a Look Forward at 20 Years of Bridge Painting Under the OSHA Lead in Construction Interim Final Rule and Other Related Standards

by Alison B. Kaelin, CQA, ABKaelin, LLC

This article provides reports on statistics and violations of OSHA’s standard for protecting construction workers from lead exposure, summarizes findings on blood lead levels and health risks related to lead exposure, reviews OSHA 29 CFR 1926.62 and other lead exposure-related regulations, and offer...

Exploring Marine Applications for Heat-Reflective Coatings

by Rob Portsmouth, Huntsman Pigments

This article describes the background of solar reflective coatings technology and discusses the potential advantages to its usage in the marine coatings sector.

Exploring Marine Applications for Heat-Reflective Coatings

by Rob Portsmouth, Huntsman Pigments

This article describes the background of solar reflective coatings technology and discusses the potential advantages to its usage in the marine coatings sector.