Comparing Test and Field Performance of Thick-Film Elastomeric Polyureas

by Dudley J. Primeaux II, PCS, CCI, Primeaux Associates, LLC

This article compares earlier accelerated weathering testing for UV stability to real time outdoor exposure of spray-applied polyurea elastomeric coating and lining systems. The article also describes several uses for the systems.

Comparing Test and Field Performance of Thick-Film Elastomeric Polyureas

by Dudley J. Primeaux II, PCS, CCI, Primeaux Associates, LLC

This article compares earlier accelerated weathering testing for UV stability to real time outdoor exposure of spray-applied polyurea elastomeric coating and lining systems. The article also describes several uses for the systems.

Renting Equipment for Painting Projects?

by Joe Maty, JPCL

The author reports on a number of views from rental company and painting contractor representatives regarding important issues related to renting equipment for protective and marine coatings projects.

Renting Equipment for Painting Projects?

by Joe Maty, JPCL

The author reports on a number of views from rental company and painting contractor representatives regarding important issues related to renting equipment for protective and marine coatings projects.