JPCL December 2009


Dry Film Thickness Measurements: How Many Are Enough?

by Rob Francis, Aurecon Australia Pty Ltd

The author provides a close look at four major international standards for measuring dry film thickness of coatings, with a focus on the number of measurements required.

Dry Film Thickness Measurements: How Many Are Enough?

by Rob Francis, Aurecon Australia Pty Ltd

The author provides a close look at four major international standards for measuring dry film thickness of coatings, with a focus on the number of measurements required.

New Waterborne Fluoropolymer Resins for Ultra-Weatherable Coatings

by Winn Darden and Bob Parker, AGC Chemicals Americas; and Naoko Sumi, Isao Kimura, Masakazu Ataku, and Takashige Maekawa, Asahi Glass Co. Ltd.

this article describes solvent-borne and waterborne FEVE resins as well as the potential uses of new FEVE dispersion resins in coatings for field application where high weathering properties are needed.

New Waterborne Fluoropolymer Resins for Ultra-Weatherable Coatings

by Winn Darden and Bob Parker, AGC Chemicals Americas; and Naoko Sumi, Isao Kimura, Masakazu Ataku, and Takashige Maekawa, Asahi Glass Co. Ltd.

this article describes solvent-borne and waterborne FEVE resins as well as the potential uses of new FEVE dispersion resins in coatings for field application where high weathering properties are needed.

PACE 2010 in Phoenix: The Advance Program

by the JPCL Staff

The advance program for PACE 2010, the joint conference of SSPC and PDCA, is published here to help protective and marine coatings personnel begin planning their activities in Phoenix, AZ. The event will be held February 7-10. Details are provided about the technical program, special events, trainin...

PACE 2010 in Phoenix: The Advance Program

by the JPCL Staff

The advance program for PACE 2010, the joint conference of SSPC and PDCA, is published here to help protective and marine coatings personnel begin planning their activities in Phoenix, AZ. The event will be held February 7-10. Details are provided about the technical program, special events, trainin...